Isoter®
Styrenic Compound (ABS-SAN-ASA) available in different grades in a wide range of melt flow rates, impact and heat resistance, in accordance with market demands and industry standards. Some products are available glass fiber reinforced; HB class and halogen-based flame retardant with UL94 certification. They can be tailor made colored, upon specific customer requirements, with high or low gloss.Nazwa | Compound | Density ISO 1183 | MFI ISO 1133 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoter® A 5 150 HT LE | ABS very high heat resistance Vicat B/50 108°C, low emission. | 1,05 g/cm3 | 6 gr/10' | 18 Kj/m2 | HB | |
Isoter® A 35 200 | ABS high flow, general purpose, good impact resistance. | 1,04 g/cm3 | 35 gr/10' | 16 Kj/m2 | HB | |
Isoter® A 30 200 FR V0 | ABS flame retardant, UL94 V0 1,5mm. | 1,20 g/cm3 | 30 gr/10' | 20 Kj/m2 | V0 YC | |
Isoter® A 20 180 | ABS medium flow, general purposes, good impact resistance. | 1,04 g/cm3 | 20 gr/10' | 17 Kj/m2 | HB | |
Isoter® A 15 250 AS | ABS medium flow, improved chemical resistance. | 1,04 g/cm3 | 20 gr/10' | 24 Kj/m2 | HB | |
Isoter® A 10 150 HT | ABS with high heat resistance Vicat B/50 105°C. | 1,05 g/cm3 | 10 gr/10' | 12 Kj/m2 | HB | |
Isoter® A 10 120 HT | ABS with high heat resistance Vicat B/50 102°C | 1,05 g/cm3 | 10 gr/10' | 12 Kj/m2 | HB | |
Isoter® A 10 100 GF17 | ABS 17% glass fiber reinforced. | 1,18 g/cm3 | 10 gr/10' | 6 Kj/m2 | HB |
Isostyr®
Styrenic Compound (PS) available in different grades, impact and heat resistance in accordance with the industry standards of household appliances and electric market. Some products are available halogen-based flame retardant. They can be tailor made colored, upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | MFI ISO 1133 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isostyr® A 10 50 | HIPS medium impact, good heat resistance and high stiffness. | 1,04 g/cm3 | 10 gr/10' | 5 Kj/m2 | HB | |
Isostyr® A 10 100 V2 | HIPS flame retardant UL94 V2 1,5 mm. | 1,13 g/cm3 | 20 gr/10' | 7 Kj/m2 | V2 |
Isoryl®
Compounds of Polyphenylene Oxide (PPO), high thermal resistance, good dimensional and hydrolytic stability. The products can be glass fiber reinforced and mineral filled; halogen-free flame retardant, UL94 certified. They can be colored upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoryl® A 20 90 GF20 W | PPO 20% glass fiber, WRAS approved. | 1,21 g/cm3 | 4500 MPa | 3 Kj/m2 | HB | |
Isoryl® A 20 75 GF20 V0 | PPO 20% glass fiber, flame retardant UL94 V0 3,00mm. | 1,24 g/cm3 | 4500 MPa | 3 Kj/m2 | V0 | |
Isoryl® A 20 10 GF30 W | PPO 30% glass fiber, WRAS approved. | 1,27 g/cm3 | 6000 MPa | 3 Kj/m2 | HB | |
Isoryl® A 137 | PPO Unfilled. | 1,06 g/cm3 | 2100 MPa | 10 Kj/m2 | HB | |
Isoryl® A 120 T20 V1 A | PPO 20% mineral filled, flame retartant UL94 V1 1,5mm. | 1,21 g/cm3 | 3600 MPa | 5 Kj/m2 | V1 YC | |
Isoryl® A 120 GF0 V0 | PPO flame retardant UL94 V0 1,5mm. | 1,10 g/cm3 | 2250 MPa | 9 Kj/m2 | V0 YC |
Isoplen®
Homopolymer and Copolymer Polypropylene Compound with high mechanical properties, developed in accordance with market demands and industry standards. Products available in a wide range of colors and certified flame retardant versions available both halogenated and halogen-free.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoplen® HK X V0 HF | Unfilled. Heat stabilized. Flame Retardant grade without halogens. | 10 g/10' | 1600 Mpa | 3,5 KJ/m2 | Classe V0 YC | |
Isoplen® H2 T V | PP homo, natural colour, heat stabilized, high flowability | 20 g/10' | 1400 MPa | 5 Kj/m2 | Classe HB | |
Isoplen® FR V2 | PP copo flame retardant low halogen content | 10 g/10' | 1400 MPa | 10 Kj/m2 | Classe V2 YC | |
Isoplen® A K Z | PP copo, high flowability | 21 g/10' | 1350 MPa | 5,6 Kj/m2 | Classe HB | |
Isoplen® A K F | PP copo, medium flowability | 13 g/10' | 1300 MPa | 11 Kj/m2 | Classe HB | |
Isoplen® A H F | PP homo, natural colour medium flowability | 12 g/10' | 1400 MPa | 3,3 Kj/m2 | Classe HB |
Isonyl®
Compounds based on polyamide 6 and 66 (PA6 – PA66), with good heat resistance and good mechanical properties. Our portfolio includes different grades, reinforced with glass and carbon fiber or mineral filled; impact modified, lubricated with Silicon, PTFE or Molybdenum disulfide; halogen or halogen-free flame retardant base, UL94 listed. Our products can be tailor made colored, upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isonyl® A 66 STZX | PA66 high impact modified. | 1,08 g/cm3 | 1800 MPa | 65 Kj/m2 | HB | |
Isonyl® A 66 STZ | PA66 impact modified. | 1,10 g/cm3 | 2000 MPa | 40 Kj/m2 | HB | |
Isonyl® A 66 ST2 | PA66 impact modified. | 1,11 g/cm3 | 2200 MPa | 30 Kj/m2 | HB | |
Isonyl® A 66 ST1 | PA66 impact modified. | 1,12 g/cm3 | 2400 MPa | 20 Kj/m2 | HB | |
Isonyl® A 66 ST | PA66 impact modified. | 1,13 g/cm3 | 2500 MPa | 9 Kj/m2 | HB | |
Isonyl® A 66 GF50 | PA66 50% glass fiber reinforced. | 1,56 g/cm3 | 14000 MPa | 13 Kj/m2 | HB | |
Isonyl® A 66 GF30 | PA66 30% glass fiber reinforced. | 1,36 g/cm3 | 8500 MPa | 12 Kj/m2 | HB | |
Isonyl® A 66 GF25 V0 | PA66 25% glass fiber, flame retardant UL94 V0 1,5 mm, with halogens. | 1,50/1,55 g/cm3 | 8500 MPa | 9 Kj/m2 | V0 | |
Isonyl® A 66 | PA66 general purpose for injection moulding. | 1,14 g/cm3 | 2900 MPa | 4 Kj/m2 | V2 | |
Isonyl® A 6 STZX | PA6 high impact modified. | 1,08 g/cm3 | 1600 MPa | 70 Kj/m2 | HB | |
Isonyl® A 6 STZ | PA6 impact modified. | 1,10 g/cm3 | 1800 MPa | 40 Kj/m2 | HB | |
Isonyl® A 6 ST2 | PA6 impact modified. | 1,11 g/cm3 | 2000 MPa | 30 Kj/m2 | HB | |
Isonyl® A 6 ST1 | PA6 impact modified. | 1,12 g/cm3 | 2300 MPa | 20 Kj/m2 | HB | |
Isonyl® A 6 ST | PA6 impact modified. | 1,13 g/cm3 | 2400 MPa | 8 Kj/m2 | HB | |
Isonyl® A 6 GS30 | PA6 30% glass beads reinforced. | 1,34 - 1,36 g/cm3 | 3150 MPa | 3 Kj/m2 | HB | |
Isonyl® A 6 GF60 | PA6 60% glass fiber reinforced. | 1,70 g/cm3 | 19000 MPa | 16 Kj/m2 | HB | |
Isonyl® A 6 GF50 | PA6 50% glass fiber reinforced. | 1,56 g/cm3 | 12000 MPa | 13 Kj/m2 | HB | |
Isonyl® A 6 GF35 | PA6 35% glass fiber reinforced. | 1,38 - 1,41 g/cm3 | 9000 Mpa | 15 KJ/m2 | HB | |
Isonyl® A 6 GF30 ST2 | PA6 30% glass fiber reinforced, impact modified. | 1,32 g/cm3 | 6800 Mpa | 17 Kj/m2 | HB | |
Isonyl® A 6 GF30 ST | PA6 30% glass fiber reinforced, impact modified. | 1,34 g/cm3 | 7300 Mpa | 14 KJ/m2 | HB | |
Isonyl® A 6 GF30 HSR | PA6 30% glass fiber reincorced, good impact resistance, heat and hydrolysis resistant. | 1,36 g/cm3 | 8000 Mpa | 12 Kj/m2 | HB | |
Isonyl® A 6 GF30 | PA 6 30% glass fiber reinforced. | 1,36 g/cm3 | 8000 Mpa | 12 Kj/m2 | HB | |
Isonyl® A 6 GF15 | PA6 15% glass fiber reinforced. | 1,21 g/cm3 | 6000 MPa | 7 Kj/m2 | HB | |
Isonyl® A 6 | PA6 general purpose for injection moulding. | 1,13 g/cm3 | 2700 MPa | 4 Kj/m2 | V2 | |
Isonyl® 6 GF30 V0 HF | PA6 30% glass fiber, flame retardant UL94 V0 1,5 mm, halogen free. | 1,41 g/cm3 | 9000 MPa | 6 Kj/m2 | V0 YC |
Isoglass®
Polypropylene Reinforced with Glass Fiber, chemically coupled or mechanical, with high thermal, impact and stiffness properties, aligned with the standards of the automotive and household appliance industries.The products are available in the color range and flame retardant grades indicated by the sectors with relevant certifications both halogenated and halogen-free.
Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoglass® XX 6014D | 30% chemically coupled glass fiber reinforced polypropylene, high stiffness. Heat stabilized. | 8 g/10' | 7000 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® SX 8022H | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. Heat stabilized. | 10 g/10' | 7700 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® SX 4015X | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045. UV stabilized. Heat stabilized. | 8 g/10' | 3800 Mpa | 6 KJ/m2 | Classe HB | |
Isoglass® SX 4010H | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to Renault-Nissan AS8. Heat stabilized. | 10 g/10' | 4000 Mpa | 8 KJ/m2 | Classe HB | |
Isoglass® ST 8020N | 40% chemically coupled glass fiber reinforced polypropylene homopolymer. UV stabilized. Heat stabilized. | 4 g/10' | 8000 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® SC 6029X | 30% chemically coupled glass fiber reinforced copolymer polypropylene. UV stabilized. Heat stabilized. | 5 g/10' | 4500 Mpa | 22 KJ/m2 | Classe HB | |
Isoglass® K 40 CGF C | 40% glass fiber reinforced copolymer polypropylene. | 4 g/10' | 6200 MPa | 15 Kj/m2 | Classe HB | |
Isoglass® K 30 CGF X | 30% glass fiber reinforced copolymer polypropylene. | 8 g/10' | 4000 Mpa | 16 KJ/m2 | Classe HB | |
Isoglass® K 20 CGF X | 20% glass fiber reinforced copolymer polypropylene. | 10 g/10' | 3400 Mpa | 13 KJ/m2 | Classe HB | |
Isoglass® HGV 6003X | 30% chemically coupled glass fiber reinforced polypropylene. High flowability. UV stabilized. Chemical Resistant. | 20 g/10' | 5500 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® HGV 6002D | 30% glass fiber homopolymer polypropylene. Heat stabilized. Detergent Resistant. | 17 g/10' | 5600 Mpa | 9,1 KJ/m2 | Classe HB YC | |
Isoglass® H3V 6009D | 30% talc filled and glass fiber reinforced polypropylene homopolymer. Heat stabilized. Detergent resistant. | 17 g/10' | 4700 Mpa | 5 KJ/m2 | Classe HB YC | |
Isoglass® H 40 CGF C | 40% glass fiber reinforced homopolymer polypropylene. | 7 g/10' | 7600 MPa | 9 Kj/m2 | Classe HB | |
Isoglass® H 30 GFT3 C HS | 30% glass fiber and talc filled polypropylene. Compliant to MS-55246 PP130.50. Heat stabilized. | 8 g/10' | 4500 Mpa | 7 KJ/m2 | Classe HB | |
Isoglass® H 30 FVL V | 30% glass fiber filled homopolymer polypropylene. | 20 g/10' | 5700 Mpa | 10 KJ/m2 | Classe HB YC | |
Isoglass® H 30 FVL C | PP homo 30% glass fiber. Heat stabilized. | 6 g/10' | 5800 MPa | 11,5 Kj/m2 | Classe HB YC | |
Isoglass® H 30 CGF X HS | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 8 g/10' | 6000 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® H 30 CGF S HS | 30% glass fiber reinforced homopolymer polypropylene. Heat stabilized. | 5 kg/10' | 6000 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® H 30 CGF F UV | 30% glass fiber reinforced homopolymer polypropylene. UV stabilized. | 13 g/10' | 5000 Mpa | 8 KJ/m2 | Classe HB | |
Isoglass® H 30 CGF C UV | 30% chemically coupled glass fiber reinforced polypropylene. Low odor and emission. Compliant to VW44045-PP10 and VW50180. UV stabilized. Heat stabilized. | 5 g/10' | 5800 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® H 30 CGF C | 30% chemically coupled glass fiber reinforced polypropylene. Heat stabilized. | 5 g/10' | 6000 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® H 30 CGF 140.80 | 30% glass fiber reinforced homopolymer polypropylene. Compliant to MS-55246 PP140.80. Heat stabilized. | 18 g/10' | 5700 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® H 25 CGF C UV | 25% chemically coupled glass fibre reinforced Polypropylene. Antistatic.UV stabilized. | 6 g/10' | 5400 Mpa | 11 KJ/m2 | Classe HB | |
Isoglass® H 20 FVL X | 20% glass fiber polypropylene. Heat stabilized. | 8 g/10' | 3900 Mpa | 7,4 KJ/m2 | Classe HB YC | |
Isoglass® H 20 CGF X HS | 20% chemically coupled glass fiber reinforced homopolymer polypropylene. Compliant to VW 44045-PP9. Heat stabilized. | 8 g/10' | 4000 Mpa | 7 KJ/m2 | Classe HB | |
Isoglass® H 20 CGF X | 20% glass fiber reinforced homopolymer polypropylene. | 8 g/10' | 3800 MPa | 8 Kj/m2 | Classe HB | |
Isoglass® EV 3007U | 15% chemically coupled glass fiber reinforced polypropylene copolymer. High flowability grade and good aesthetical appearance. UV stabilized. | 18 g/10' | 2600 Mpa | 12 KJ/m2 | Classe HB | |
Isoglass® 4F 4030U | 22% chemically coupled glass fiber and mineral filled reinforced polypropylene copolymer. Good stiffness and impact strenght balance combined with high flowability. UV stabilized. | 14 g/10' | 3200 Mpa | 9 KJ/m2 | Classe HB |
Isoglass® XT
High Performance Glass Fiber chemically coupled Polypropilene. The properties guaranteed by this range of PPGF are aligned with high performance polymers, however, guaranteeing the characteristics of the PP. These products provide good combination of thermal and mechanical stress combined with high rigidity.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoglass® XT 8008H | 40% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 5 g/10' | 10000 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® XT 7001H | 35% chemically coupled glass fiber reinforced polypropylene homopolymer. Low flowability grade. Heat stabilized. | 3 g/10' | 8000 Mpa | 12 KJ/m2 | Classe HB | |
Isoglass® XT 6010H | 30% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness and low emission. | 6 g/10' | 8400 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® XT 6001H | 30% chemically coupled high performance glass fiber reinforced polypropylene. Heat stabilized. | 3,5 g/10' | 6500 Mpa | 10 KJ/m2 | Classe HB | |
Isoglass® XT 6001D | 30% chemically coupled high performance glass fiber reinforced polypropylene compound. | 5 g/10' | 6800 Mpa | 11 KJ/m2 | Classe HB YC | |
Isoglass® XT 4007U | 20% chemically coupled high performance reinforced polypropylene homopolymer. High stiffness and low emission. Compliant to DBL 5430. UV stabilized. | 7 g/10' | 6100 Mpa | 9 KJ/m2 | Classe HB | |
Isoglass® XT 4001D | 20% chemically coupled glass fiber reinforced polypropylene. | 7 g/10' | 4000 Mpa | 7 KJ/m2 | Classe HB YC | |
Isoglass® XT 1003H | 50% chemically coupled high performance glass fiber reinforced polypropylene homopolymer. High stiffness grade. Heat stabilized. | 3,5 g/10' | 13000 Mpa | 9 KJ/m2 | Classe HB |
Isoglass® LFT
Polypropylene Pultrusion Compound with long fiber for applications with high dimensional stability and high thermal and mechanical performance. The use of PP LFT is mainly required for structural applications where the orientation of long fibers modifies the anisotropic effect, increasing dimensional stability obtaining applications with very high stiffness. The product range is available in different fiber contents even at high concentrations.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoglass® LFT 1001H | PP homo 50% long glass fiber, heat stabilized. | / | 10500 MPa | 29 Kj/m2 | Classe HB | |
Isoglass® LFT LFT 0603H | 30% chemically coupled long glass fiber reinforced polypropylene compound with very high mechanical properties and heat stabilized. | / | 6300 Mpa | 21 Kj/m2 | Classe HB |
Isoform®
Compounds based on copolymer or homopolymer acetal resin (POM) with high stiffness and an outstanding wear resistance. Our products are available glass fiber reinforced; impact modified and lubricated with Silicon, PTFE or Molybdenum Disulfide. They can be tailor made colored, upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | MFI ISO 1133 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoform® A K 45 | POM COP general purpose, very low viscosity. | 1,41 g/cm3 | 45 gr/10' | 4 Kj/m2 | HB | |
Isoform® A K 27 | POM COP general purpose, low viscosity. | 1,41 g/cm3 | 27 gr/10' | 6 Kj/m2 | HB | |
Isoform® A K 13 | POM COP general purpose, medium viscosity. | 1,41 g/cm3 | 13 gr/10' | 6 Kj/m2 | HB | |
Isoform® A K 09 STZ | POM COP impact modified. | 1,37 g/cm3 | 11 gr/10' | 15 Kj/m2 | HB | |
Isoform® A K 09 GF25 | POM COP 25% glass fiber. | 1,59 g/cm3 | 4 gr/10' | 6 Kj/m2 | HB | |
Isoform® A K 09 | POM COP general purpose, medium viscosity. | 1,41 g/cm3 | 9 gr/10' | 7 Kj/m2 | HB | |
Isoform® A K 03 | POM COP general purpose, high viscosity. | 1,41 g/cm3 | 3 gr/10' | 8 Kj/m2 | HB |
Isoflex®
Copolymer Polypropylene, unfilled and not stabilized.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoflex® C800 | Polypropylene copolymer. | 6 g/10' | 800 Mpa | 45 KJ/m2 | / |
Isofil®
Standard and High Performance Modified Polypropylene with different mineral fillers (T/TC/CaCO3/BaSO4/Mica) in accordance with market demands and industry standards. Products with application features in colors and specifications developed with customers. Certified flame retardant versions are available both halogenated and halogen-free.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isofil® SW 4909U | 20% talc filled copolymer polypropylene. Impact modified grade with high flowability. UV stabilized. | 40 g/10' | 1500 Mpa | 40 KJ/m2 | Classe HB | |
Isofil® SV 4205Y | 20% talc filled polypropylene copolymer. Good flowability and stiffness. UV stabilized. Scratch Resistant. | 16 g/10' | 2300 Mpa | 6 KJ/m2 | Classe HB | |
Isofil® SV 4118X | 20% talc filled homopolymer polypropylene. Compliant to TL 52658-WD01. UV stabilized. Heat stabilized. | 16 g/10' | 2800 Mpa | 2,5 KJ/m2 | Classe HB | |
Isofil® SF 4501Y | 20% talc filled copolymer polypropylene. Impact modified grade. UV stabilized. Scratch Resistant. | 14 g/10' | 1900 Mpa | 20 KJ/m2 | Classe HB | |
Isofil® SF 4303U | 20% talc filled copolymer polypropylene with good stiffness and impact resistance. UV stabilized. | 15 g/10' | 1800 Mpa | 15 KJ/m2 | Classe HB | |
Isofil® RV 4603S | 20% talc filled impact modified polypropylene. Compliant to TL 52388-F. UV stabilized. Scratch Resistant. | 18 g/10' | 2000 Mpa | 35 KJ/m2 | Classe HB | |
Isofil® RF 3403Y | 15% talc filled polypropylene copolymer. Impact modified. High fluidity. Low CLTE. UV stabilized. Scratch Resistant. | 15 g/10' | 1700 Mpa | 25 KJ/m2 | Classe HB | |
Isofil® PZ 8103H | 40% talc filled polypropylene homopolymer. Heat stabilized. | 20 g/10' | 4300 Mpa | 3 KJ/m2 | Classe HB | |
Isofil® PF 4102H | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6 and WSS-M4D729-B1. Heat stabilized. | 12 g/10' | 2800 Mpa | 3 KJ/m2 | Classe HB | |
Isofil® MZ 3506Y | 17% talc filled copolymer polypropylene. Good flowability. Low emission. UV stabilized. Heat stabilized. Scratch Resistant. | 22 g/10' | 2000 Mpa | 25 KJ/m2 | Classe HB | |
Isofil® MZ 2102H | 10% talc filled homopolymer polypropylene. Low emission grade. | 25 g/10' | 2350 Mpa | 3,5 KJ/m2 | Classe HB | |
Isofil® MY 2205Y | 10% talc filled copolymer polypropylene. Low emission grade. Scratch Resistant. | 25 g/10' | 1600 Mpa | 18 KJ/m2 | Classe HB | |
Isofil® MV 4509Y | 20% talc filled polypropylene copolymer. Impact modified. UV stabilized. Scratch Resistant. | 26 g/10' | 1900 Mpa | 30 KJ/m2 | Classe HB | |
Isofil® MF 4124S | 20% talc filled polypropylene compound. It exhibits high stiffness and low emission properties. Scratch Resistant. | 15 g/10' | 2700 Mpa | 4 KJ/m2 | Classe HB | |
Isofil® MF 3604Y | 16% talc filled polypropylene. Impact resistance grade. UV stabilized. Scratch Resistant. | 14 g/10' | 1500 Mpa | 30 KJ/m2 | Classe HB | |
Isofil® MC 4214Y | 20% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 8 g/10' | 2300 Mpa | 7 KJ/m2 | Classe HB | |
Isofil® KPZ 4001D | 20% talc filled copolymer polypropylene. Heat stabilized. | 20 g/10' | 2400 Mpa | 4,7 KJ/m2 | Classe HB YC | |
Isofil® KGF 4002U | 21,5% talc filled copolymer polypropylene. UV stabilized. | 12 g/10' | 2000 Mpa | 4 KJ/m2 | Classe HB | |
Isofil® K 40 TP V | PP copo 40% talc | 20 g/10' | 3400 MPa | 4,2 Kj/m2 | Classe HB | |
Isofil® K 40 T xxx HB | 40% talc filled copolymer polypropylene. Heat stabilized. | 8 g/10' | 3800 Mpa | 2,6 KJ/m2 | Classe HB YC | |
Isofil® K 40 T | 40% talc filled polypropylene. | 7 g/10' | 4200 Mpa | 2,6 KJ/m2 | Classe HB | |
Isofil® K 30 T 60.90L | 30% talc filled copolymer polypropylene. UV stabilized. | 16 g/10' | 2300 Mpa | 9 KJ/m2 | Classe HB | |
Isofil® K 30 T 50.200LCE SR AF | 30% talc filled copolymer polypropylene. High impact. Scratch resistant. High fluidity. UV stabilized. | 33 g/10' | 1700 Mpa | 20 KJ/m2 | Classe HB | |
Isofil® K 20 TP X | PP copo 20% talc | 10 g/10' | 2000 MPa | 7 Kj/m2 | Classe HB | |
Isofil® K 20 T xxx HB | 20% talc filled copolymer polypropylene. | 16 g/10' | 2300 Mpa | 6,5 KJ/m2 | Classe HB YC | |
Isofil® K 20 T 50.400LCE SR AF | 17% talc filled copolymer polypropylene. Low CLTE and scratch resistant. UV stabilized. | 32 g/10' | 1450 Mpa | 40 KJ/m2 | Classe HB | |
Isofil® K 20 T 48.450 AFU | 20% talc filled copolymer polypropylene. Impact modified and scratch resistant. UV stabilized. | 19 g/10' | 1700 Mpa | 45 KJ/m2 | Classe HB | |
Isofil® K 10 T 53.180U | 13% talc filled copolymer polypropylene. UV stabilized. Scratch Resistant. | 15 g/10' | 1650 Mpa | 18 KJ/m2 | Classe HB | |
Isofil® K 10 T 46.400 AFU | 10% talc filled copolymer polypropylene. Scratch resistant. UV stabilized. | 22 g/10' | 1300 Mpa | 40 KJ/m2 | Classe HB | |
Isofil® K 0 T xxx HB | Copolymer polypropylene. | 17 g/10' | 1200 Mpa | 7,9 KJ/m2 | Classe HB YC | |
Isofil® HZ 9101D | 40% talc filled homopolymer polypropylene. Good flowability. | 23 g/10' | 4100 Mpa | 2,5 KJ/m2 | Classe HB | |
Isofil® HK 50 C2 V | 50% calcium carbonate homopolymer polypropylene. Heat stabilized. | 18 g/10' | 3100 Mpa | 2,5 KJ/m2 | Classe HB YC | |
Isofil® HK 50 2FH0 | 50% calcium carbonate filled polypropylene. | 20 g/10' | 2800 Mpa | 3,5 KJ/m2 | Classe HB | |
Isofil® HK 40 TVH0 | 40% talc filled copolymer polypropylene. | 18 g/10' | 4000 Mpa | 3 KJ/m2 | Classe HB YC | |
Isofil® HK 40 TTH0 | 40% talc filled homopolymer polypropylene. Heat stabilized. | 4 g/10' | 3800 Mpa | 2,4 KJ/m2 | Classe HB YC | |
Isofil® HK 40 5FH0 | 40% calcium carbonate polypropylene. | 13 g/10' | 2500 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 40 2FH0 | 40% calcium carbonate filled polypropylene. Heat stabilized. | 13 g/10' | 2500 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 35 GVH0 | 35% talc filled copolymer polypropylene. | 21 g/10' | 3100 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TXH0 | 30% talc filled polypropylene. Heat stabilized. | 8 g/10' | 3300 Mpa | 2,7 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TVH2 | 30% talc filled polypropylene. | 16 g/10' | 3200 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TVH0 | 30% talc filled homopolymer polypropylene. | 20 g/10' | 3400 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TTH1 | 30% talc filled polypropylene. UV stabilized. Heat stabilized. | 3 g/10' | 3400 Mpa | 2,3 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TTH0 | 30% talc polypropylene. | 4 g/10' | 3300 Mpa | 3,1 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TSH1 | 30% talc filled polypropylene homopolymer. Heat stabilized. | 3 g/10' | 3500 Mpa | 5 KJ/m2 | Classe HB YC | |
Isofil® HK 30 TFH2 | 30% talc filled polypropylene. | 14 g/10' | 34600 Mpa | 3,8 KJ/m2 | Classe HB YC | |
Isofil® HK 25 TVH0 | 25% talc filled copolymer polypropylene. | 23 g/10' | 1800 Mpa | 7 KJ/m2 | Classe HB YC | |
Isofil® HK 25 GVH1 | 25% talc copolymer polypropylene. Heat stabilized. | 17 g/10' | 2000 Mpa | 12,9 KJ/m2 | Classe HB YC | |
Isofil® HK 25 GVH | 25% talc filled copolymer polypropylene. | 16 g/10' | 2200 Mpa | 5,1 KJ/m2 | Classe HB YC | |
Isofil® HK 25 6VH | 25% talc-calcium carbonate filled polypropylene. | 16 g/10' | 2400 Mpa | 5 KJ/m2 | Classe HB YC | |
Isofil® HK 20 TP F HS | 20% talc filled copolymer polypropylene. | 12 g/10' | 2200 Mpa | 6 KJ/m2 | Classe HB | |
Isofil® HK 20 TFHH | 20% talc filled polypropylene. Heat stabilized. Detergent Resistant. | 5 g/10' | 2200 Mpa | 3,9 KJ/m2 | Classe HB YC | |
Isofil® HK 20 TFH0 | 20% mineral filled polypropylene. Heat stabilized. | 13 g/10' | 2300 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 20 TCH0 | 20% mineral filled polypropylene. Heast stabilized. | 6 g/10' | 2300 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® HK 20 T V0 | 20% talc filled copolymer polypropylene. Heat stabilized. Flame Retardant grade With halogens | 6 g/10' | 2900 Mpa | 3,5 KJ/m2 | Classe HB | |
Isofil® HK 20 2VH0 | 20% calcium carbonate polypropylene. Heat stabilized. | 16 g/10' | 1850 Mpa | 2,4 KJ/m2 | Classe HB YC | |
Isofil® HK 10 TVHM | 10% micro talc filled polypropylene. | 20 g/10' | 2400 MPa | 4 Kj/m2 | Classe HB YC | |
Isofil® HF 6205X | 30% talc filled copolymer polypropylene. UV stabilized. Heat stabilized. | 14 g/10' | 2300 Mpa | 6 KJ/m2 | Classe HB | |
Isofil® HF 2206H L | 10% talc filled polypropylene copolymer. Heat stabilized. Laserable. | 12 g/10' | 1500 Mpa | 8 KJ/m2 | Classe HB | |
Isofil® H 40 TP F | PP homo 40% talc | 12 g/10' | 4000 MPa | 2,4 Kj/m2 | Classe HB | |
Isofil® H 40 TG X HS | 40% talc filled homopolymer polypropylene. Compliant to VW 44045-PP8. Heat stabilized. | 15 g/10' | 4000 Mpa | 2,5 KJ/m2 | Classe HB | |
Isofil® H 40 TG S HS | 40% talc filled polypropylene homopolymer. | 10 kg/10' | 4100 Mpa | 3,5 KJ/m2 | Classe HB | |
Isofil® H 40 C2 X | 40% calcite filled homopolymer polypropylene. | 9 g/10' | 2400 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® H 40 C2 F | 40% calcium carbonate filled homopolymer polypropylene. | 13 g/10' | 2500 Mpa | 3,3 KJ/m2 | Classe HB YC | |
Isofil® H 20 TP X | PP homo 20% talc natural colour | 9 g/10' | 2600 MPa | 3 Kj/m2 | Classe HB | |
Isofil® H 20 TP F HS | 20% Talc filled polypropylene homopolymer. Low emission. Compliant to VW44045-PP6.Heat stabilized. | 12 g/10' | 2800 Mpa | 3 KJ/m2 | Classe Hb | |
Isofil® H 20 T F UV | 20% talc filled homopolymer polypropylene. UV stabilized. | 15 g/10' | 2600 Mpa | 2,5 KJ/m2 | Classe HB |
Isodur®
Polyesters compounds (PBT) available in different grades, high heat and chemical resistant, good dimension stability. Our products can be glass fiber reinforced; halogen-based flame retardant, UL94 certified. They can be tailor made colored, upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isodur® A 15 10 GF30 | PBT 30% glass fiber reinforced. | 1,56 g/cm3 | 8500 MPa | 8 Kj/m2 | HB | |
Isodur® A 15 10 GF20 | PBT 20% glass fiber reinforced. | 1,45 g/cm3 | 5500 MPa | 7 Kj/m2 | HB | |
Isodur® 15 10 GF20 V0 | PBT 20% glass fiber reinforced, flame retardant UL94 V0 1,5mm. | 1,57/1,59 g/cm3 | 7000 MPa | 7 Kj/m2 | V0 YC |
Isoclear®
Polycarbonate Compounds (PC) offering a good combination of toughness, impact strength and high heat resistance. Our products can be glass fiber reinforced and impact modified. They are UL94 certified for flame retardance, available both halogenated and halogen-free base. They can be colored upon specific customer requirements, also in transparent colors.Nazwa | Compound | Density ISO 1183 | MFI ISO 1133 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoclear® A 20 60 | PC low viscosity, good mechanical and high heat resistance, for transparent and solid colors. | 1,2 g/cm3 | 20 gr/10' | 60 Kj/m2 | HB | |
Isoclear® A 10 60 GF10 V0 | PC 10% glass fiber reinforced, flame retardant, with halogens, UL94 V0 1,6 mm. | 1,26 - 1,30 g/cm3 | 10 gr/10' | 7 Kj/m2 | V0 YC | |
Isoclear® A 10 60 GF0 V0 | PC flame retardant, with halogens, UL94 V0 1,6 mm. | 1,20 g/cm3 | 10 gr/10' | 50 Kj/m2 | V0 YC | |
Isoclear® A 10 60 | PC medium viscosity, good mechanical and high heat resistance, for transparent and solid colors. | 1,2 g/cm3 | 10 gr/10' | 60 Kj/m2 | HB |
Isoblend®
Compounds available in a wide range of different polymers alloys. Our portfolio includes reinforced grades; halogen or halogen-free flame retardant grades, UL94 certified. They can be tailor made colored, upon specific customer requirements.Nazwa | Compound | Density ISO 1183 | Vicat B/50 ISO 306 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoblend® B 65 | Unfilled PC/ABS alloy. Natural colour. | 1,12 g/cm3 | 120 °C | 40 Kj/m2 | HB | |
Isoblend® A 85 AF UV | Blend PC/ABS, high fluidity, UV stabilized. | 1,15 g/cm3 | 129 °C | 50 KJ/m2 | HB | |
Isoblend® A 85 | Blend PC/ABS general purpose, good flow properties, good impact and heat resistance. | 1,15 - 1,16 g/cm3 | 129 °C | 55 Kj/m2 | HB | |
Isoblend® A 65 PG | Blend PC/ABS, suitable for electroplating application. | 1,11 g/cm3 | 126 °C | 50 KJ/m2 | HB | |
Isoblend® A65 GF20 | Blend PC/ABS 20% glass fiber reinforced. | 1,29 g/cm3 | 130 °C | 9 KJ/m2 | HB | |
Isoblend® A65 GF17 | Blend PC/ABS, 17% glass fiber reinforced. | 1,29 g/cm3 | 127 °C | 10 KJ/m2 | HB | |
Isoblend® A 65 AF UV | Blend PC/ABS, high fluidity, UV stabilized. | 1,12 g/cm3 | 118 °C | 30 KJ/m2 | HB | |
Isoblend® A 65 | Blend PC/ABS general purpose, good flow properties and good impact resistance. | 1,13 - 1,15 g/cm3 | 118 °C | 35 Kj/m2 | HB | |
Isoblend® A 50 UV | Blend PC/ABS, UV stabilized. | 1,12 g/cm3 | 120 °C | 50 KJ/m2 | HB | |
Isoblend® A 45 PG | Blend ABS/PC, suitable for electroplating application. | 1,08 g/cm3 | 110 °C | 45 KJ/m2 | HB | |
Isoblend® A 45 | Blend ABS/PC general purpose, good flow properties. | 1,10 - 1,12 g/cm3 | 110 °C | 30 Kj/m2 | HB | |
Isoblend® A 40 200 V0 | Blend PC/ABS flame retardant UL94 V0 1,5mm, halogen free. | 1,17 g/cm3 | 105 °C | 30 Kj/m2 | V0 YC | |
Isoblend® A 20 500 V0 | Blend PC/ABS flame retardant UL94 V0 1,5mm, halogen free. | 1,17 g/cm3 | 110 °C | 50 KJ/m2 | V0 YC |
Nazwa | Compound | Density ISO 1183 | MFI ISO 1133 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Isoblend® AS 15 15 V0 UV | Blend PC/ASA flame retardant UL94 V0 3,00mm, UV resistance. | 1,17 g/cm3 | 13 gr/10' | 15 Kj/m2 | V0 | |
Isoblend® AS 15 15 UV | Blend PC/ASA good UV and weathering resistance, high heat resistance, good impact strength. | 1,13 - 1,16 g/cm3 | 15 gr/10' | 20 Kj/m2 | HB |
Green Isonyl®
Polyamide 6 with Glass Fiber reinforcement formulated with partial use of post-industrial compound and recycled feedstocks. The products are available in accordance with some standards recently introduced by the automotive and tools sectors in black colors.Nazwa | Compound | Density ISO 1183 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Green Isonyl® I 66 GF25 GW | 25% glass fiber reinforced polyamide 66. Flame retardant grade with GWFI 850°C on 2 mm thickness. Recycled content. | / | 7500 MPa | 7 KJ/m2 | / |
Green Isoglass®
Polypropylene with Glass Fiber reinforcement formulated with partial use of post-industrial and post consumer raw materials. The products are available in accordance with some standards recently introduced by the automotive and appliance sectors.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Green Isoglass® H 40 CGF X HS | 40% glass fiber reinforced polypropylene. Industrial quality. Heat stabilized. | 10 g/10' | 6000 MPa | 9 Kj/m2 | Classe HB | |
Green Isoglass® H 30 CGF C HS | 30% chemically coupled glass fiber reinforced polypropylene with 30% circular polymer source. Heat stabilized. | 6 g/10' | 4900 MPa | 9 Kj/m2 | Classe HB |
Green Isofil®
Polypropylene with Mineral Filler formulated with partial quantities of post-industrial and post-consumer raw materials. The products are available in accordance with some standards recently introduced by the automotive and appliance sectors.Nazwa | Compound | MFI ISO 1133 | MEF ISO 178 | Izod Notched ISO 180/1A | Flammability UL94 | |
---|---|---|---|---|---|---|
Green Isofil® K 30 T T HS | 30% talc filled polypropylene copolymer. Industrial quality. Heat stabilized. | 3 g/10' | 2200 MPa | 6 Kj/m2 | Classe HB | |
Green Isofil® HK 40 C F | PP copo 40% calcium carbonate, heat stabilized, detergent resistant. | 20 g/10' | 1900 MPa | 3,3 Kj/m2 | Classe HB |